Organisation/Company ALMA MATER STUDIORUM - UNIVERSITA' DI BOLOGNA - - DIPARTIMENTO DI INGEGNERIA INDUSTRIALE Research Field Engineering Researcher Profile Recognised Researcher (R2) Leading Researcher (R4) First Stage Researcher (R1) Established Researcher (R3) Application Deadline 24 Aug 2026 - 23:59 (UTC) Country Italy Type of Contract To be defined Job Status Not Applicable Is the job funded through the EU Research Framework Programme? Not funded by a EU programme Is the Job related to staff position within a Research Infrastructure? No

Offer Description

The activity is focused on the study of cast aluminum alloys for engine applications, with the aim of supporting material selection, process optimization, and heat treatment design through compositional, microstructural, mechanical, and fractographic characterization of engine components. The activity is carried out in the framework of the development of high-performance and high-reliability components for the automotive sector.

- Italy

Eligibility of fellows: country/ies of residence:

- All

Eligibility of fellows: nationality/ies:

#J-18808-Ljbffr

Technical Compliance

26 ago - Mantova
Michael Page International Italia

Brand Experience Sales Associate

26 ago - Belluno
Pvh Italy

Ricevi nuove offerte di lavoro

Crea una Job Alert gratuita per chemical, microstructural, mechanical, and fractographic characterization of aluminum alloy castings for engine components / italia

Technical Compliance

26 ago - Perugia
Michael Page International Italia

ERP Team Leader

26 ago - Salerno
DRS RADA TECHNOLOGIES